Eigentum | Einheit | Testmethode | Typische Werte | ||
Physisch | |||||
Dicke | Mikron | Intern | 20 | 25 | 30 |
Ertrag | m2/kg | Intern | 54, 9 | 44 | 36, 6 |
Dichte | G/cm3 | Intern | 0, 91 | 0, 91 | 0, 91 |
Mechanisch | |||||
Zugfestigkeit MD | Kg/cm2 | ASTM-D-882 | 500 | 520 | 525 |
TD | Kg/cm2 | ASTM-D-882 | 400 | 415 | 420 |
Ultimative Dehnung MD | % | ASTM-D-882 | 550 | 580 | 600 |
TD | % | ASTM-D-882 | 650 | 685 | 695 |
Oberfläche | |||||
Koeffizient Statisch | - | ASTM-D-1894 | 0, 35 | 0, 35 | 0, 35 |
Reibungsdynamik | - | ASTM-D-1894 | 0, 3 | 0, 3 | 0, 3 |
Netzspannung | Dyne/cm | ASTM-D-2578 | 38 | 38 | 38 |
Reißfestigkeit | G/Mikron | ASTM-D-2578 | 5, 2 | 5, 4 | 5, 5 |
Optisch | |||||
Dunst | % | ASTM-D-1003 | 3, 6 | 4, 2 | 4, 6 |
Transmissionsgrad | % | ASTM-D-1003 | 90 | 89 | 89 |
Thermischer MD Schrumpfung TD | % | ASTM-D-1204 | 1 | 0, 9 | 0, 85 |
1, 5 | 1, 46 | 1, 35 | |||
Wasserdampfdurchlässigkeit | G /(m2•24 h) 40 Celsius | ASTM E 96 | 1, 32 | 1, 12 | 0, 98 |
Sauerstofftransmissionsrate | Ml /m2 •24 h•0, 1MPa | ASTM D 3985 | 35 | 31 | 26 |
Aluminiumschicht | |||||
Dicke | A | Intern | 300-500 | 300-500 | 300-500 |
Gleichmäßigkeit | % | Intern | 96 | 96 | 96 |
Blechwiderstand | - | ||||
Haftfähigkeit | % | GB | 94 | 94 | 94 |