Chemical component:95%ZrO2,5%Y2O3 | ||
Density | g/cm3 | 6.02 |
Water absorption | % | 0 |
Sintering temperature | C | 1540 |
Hardness | HV | 1360 |
Flexural strength | Mpa | 1400 |
Compressive strength | Mpa | 2500 |
Fracture toughness | Mpa.m3/2 | 7 |
Thermal expansion coefficient | /C | 10.2*10-6 |
Thermal shock resistance | T(C) | 360 |
Thermal conductivity | W/m.k(25-300C) | 2 |