Grade | Density g/cm3 | Hardnes HRA | T.R.S Mpa | Performance&application recommended |
YG6 | 14.90 | 90.5 | 2400 | Good wear resistance,suitable for machining hard, rawwood,aluminum section bar,brass rod and cast iron. |
YG6X | 14.85 | 92.5 | 2000 | Wear resistance higher than YG6,suitable for machining hard,rawwood,aluminum section bar,brass rod and cast iron. |
YG8 | 14.7 | 89.8 | 2800 | High wear and impact resistance,suitable for machining dry wood,soft wood and non-ferrous metal section bar |
YS2T | 14.25 | 92.0 | 2400 | Fine grain alloy,with high wear resistance,bending strength,bonding resistance and thermal strength.lt is suitable formachining refractory alloys,stainless steel,high manganesesteel,etc. |
YL10.2 | 14.45 | 91.8 | 3000 | Wear resistance and strength comparatively higher,suitable for machining cast iron,non-ferrous metal and non-metallid materials |
W(mm) | T(mm) | L(mm) | W(mm) | T(mm) | L(mm) | |
3~10 | 1.2~10 | 10~800 | 50~60 | 1.2~10 | 10~800 | |
10~20 | 1.2~10 | 10~800 | 60~70 | 1.2~10 | 10~800 | |
20~30 | 1.2~10 | 10~800 | 70~80 | 1.2~10 | 10~800 | |
40~50 | 1.2~10 | 10~800 | 80~100 | 1.2~10 | 10~800 | |
17 | 1.2~10 | 10~800 | customize | customize | customize |