In addition to its decorative effect, the coating quickly expands when encountering high-temperature flames to form a uniform and dense carbonized layer that is dozens of times the coating. The carbonized layer has low thermal conductivity, good structural strength, and resistance to high-temperature flame shear impact , Which can effectively prevent the transfer of high temperature to the steel components at the fire site. After the building's load-bearing steel components are sprayed with reliable fireproof coatings, the losses caused by accidental fires can be minimized (such as fighting for valuable time, relatively safe fighting conditions, etc.).
Fire resistance limit | 0.5-3 hours |
Coating thickness | 1.5-3mm for each time |
Construction process | Pretreatment and cleaning of the surface of the steel structure; After spraying to standard thickness, apply special top coat (colorable) .The interval between front and rear coatings is controlled at more than 24 hours |
Main ingredients | Inorganic thermal insulation materials |
Material | cement, vermiculite, perlite, fiber, river sand, calcium carbonate, talc powder, bentonite, viscosify instant powder |
Features | eco-friendly; odorless; non-toxic, anti-aging, reliable durability |
Application | Building, indoor etc. |