UNS | W.Nr |
N08825 | 2.4858 |
Alloy | % | Ni | Cr | Fe | C | Mn | Mn | Cu | Mo | Al | Ti | P | S |
Min | 38 | 19.5 | balance | 1.5 | 2.5 | 1 | 0.6 | ||||||
825 | Max | 46 | 23.5 | balance | 0.05 | 1 | 0.5 | 3 | 3.5 | 0.2 | 1.2 | 0.02 | 0.03 |
Density | 8.1 g/cm³ |
Melting point | 1370-1400°C |
Alloy state | Tensile strength Rm N/mm² | Yield strength R P0. 2N/mm² | Elongation A 5 % | Brinell hardness HB |
825 | 550 | 220 | 30 | ≤200 |