PE Film (0.1 mm) | Test Method | Unit | Test Date |
1% Forward Cut | ASTM D 882 | Mpa | >145 |
Tensile Strength at Break Forward | ASTM D 882 | Mpa | >30 |
Hood tear strength | ExxonMobil Method | OK | |
Elmendorf tear strength (longitudinal) | ASTM D 1922 | >7.5 | |
Elmendorf tear strength (transverse) | ASTM D 1003 | >12.5 | |
Shrinkage | % | >60 |