Item | Unit | GPSN |
Density | g/cm3 | 3.20±0.02 |
Elastic Modulus | Gpa | 300~320 |
Crushing Load Ratio | (25ºC)% | 30~35 |
Hardness | (HV)(Gpa) | 1600-1800 |
Fracture Toughness | Mpa.m 1/2 | 6.0~7.0 |
Bending Strength | Mpa | 650~750 |
Poisson's Ratio | 0.25 | |
Coefficient of Heat Expansion | 10-6K-1 | 3.0~3.2 |
Weber Modulus | 10~12 | |
Thermal Conductivity | W.(M.K) -1 | 15~20 |
Specific Resistivity | 1018 | |
Magnetic | No |
Item | Unit | GPSN |
Density | g/cm3 | 3.2~3.4 |
Bending strength | Mpa | ≥900 |
Fracture toughness | Mpa.m 1/2 | 6~8 |
Hardness (HV) | Gpa | 15~17 |
Thermal conductivity | W/m.k | 23~25 |
Thermal expansion coefficient | ×10-6/ºC(0~1400ºC) | 2.95~3 |