Properties | Typical Data UL 1441ASTM D 350ASTM D 372 | Test Method |
Continuous operating temperature | -10ºC~200ºC | |
Voltage withstand(Rated voltage,600V,A level) | Average value≥7000V,single value>5000V | |
Voltage withstand(Rated voltage300V,B level) | Average value≥4000V,single value>2500V | |
Voltage after heat ageing(Rated voltage600V,A level) | Average value>50of that before heat ageing | 265ºC×168h |
Voltage after heat ageing(Rated voltage300V,Blevel) | Average>2500 | 265ºC×168h |
Cold flexibility | No cracking | -10ºC×1h |
Horizontal firing | No flame propagation,no igniting cotton VW-1 | |
Vertical burning | WV-1 | |
Volume resistivity | ≥1011Ω.cm | |
Hydrolysis resistance | NO going tacky,no deforming,no softening |
Size | Standard size(mm) | Standard package (m/spool) | ||
Inner diameter | MinWall Thickness | Average thickness | ||
1.0 | 1.0±0.3 | 0.60 | 0.80±0.05 | 200 |
2.0 | 2.0±0.3 | 0.60 | 0.80±0.05 | 200 |
3.0 | 3.0±0.3 | 0.80 | 1.0±0.05 | 100 |
4.0 | 4.0±0.3 | 0.8 | 1.0±0.05 | 100 |
5.0 | 5.0±0.4 | 0.8 | 1.0±0.05 | 100 |
6.0 | 6.0±0.4 | 1.0 | 1.2±0.05 | 100 |
7.0 | 7.0±0.4 | 1.0 | 1.2±0.05 | 50 |
8.0 | 8.0±0.5 | 1.0 | 1.2±0.05 | 50 |
9.0 | 9.0±0.5 | 1.2 | 1.5±0.05 | 50 |
10.0 | 10.0±0.5 | 1.2 | 1.5±0.05 | 50 |