Pattern glass/Figured glass
Glass thickness
3mm,4mm,5mm,5.5mm,6mm,8mm,10mm,12mm etc
Glass color
Bule,Bronze,Clear,Green,Grey etc
Size
2000*1500mm,2134*1524mm, 2200*1900mm, 2440*1830mm, 2500*2000mm, 2520*1530mm, 2520*1860mm, 2520*1880mm, 2550*1880mm etc. The size
can be customized according to your request.
Application
1. Windows,doors,
2. Skylights and canopies,
3. Glass stairs,balustrades,
4. Automotive windshield,
5. Facades and curtain walls
Features
1.Rich and colorful pattern designs provide unique decorative results: or obscure and quiet, or sparkling and lively, or serious
and elegant, or bold and generous; 2.Stereoscopic effect patterned and never fade; 3.Each distinctive pattern offers a different
level of obscuration,providing privacy without sacrificing natural light; 4.Can be cut, ground, drilled, tempered, laminated and
other deep-processing glass products
Application
1.Furniture & show shelves. 2.Areas where visual screen is required, like bathrooms, doors and windows. 3.Decorative illuminations
etc.
Detailed Photos

Certifications

Packaging & Shipping

Factory

FAQ

Q1: How to judge the quality of float glass?
A1: Flatness, transparency, colorless, impurities, bubbles, etc.

Q2: How to reduce the self-implosion?
A2: The high quality float method is used for hot dip treatment, edge treatment and proper stress intensity. Pay attention to avoid side collision of glass during installation.

Q3: Scope of use of toughened glass?
A3: Safety is not involved in some parts of the building, but it is necessary to install toughened glass to improve the compressive strength and explosion-proof capacity,not to endanger the person safety

Q4: When toughened glass is broken, is the grain smaller the better?
A4: No, the smaller the particle, the easier it is to explode.

Q5: Can toughened glass and semi-toughened glass be made into laminated glass?
A5: Can't. The national standard stipulates: the glass that stresses the difference cannot make laminated glass, because in use process, the pressure that two pieces of glass bears is different.

Q6: Whether the laminated glass can fire, can the sound insulation?
A6: No, the smaller the particle, the easier it is to explode.

Q7: How many uv low-e glass can reduce?
A7: It is not fireproof glass, but has certain fireproof ability, also can soundproof, laminated glass is inside whole sound wave frequency range, in control noise is very good.

Q8: Does the air in the insulating glass do not oxidize the membrane?
A8: No, because there is a molecular sieve in the insulating glass, and the molecular sieve always keeps the air dry, so the
membrane is not oxidized.

Q9: How much ultraviolet radiation can low-e glass reduce?
A9: It can reduce uv by 14% compared to heat reflecting glass. That's a 25 percent reduction in uv radiation compared to white glass.