Professional Vendor OEM ODM No Ripple AB Glue Natural Defoaming Adhesive Clear Epoxy Resin For Wood River TableItem (HF402) | Epoxy Resin(A ) | Epoxy Resin(B ) |
Color | Transparent Liquid | Transparent Liquid |
Viscosity@25ºC(mpa.s) | 380-450 | 30-40 |
Mix Ratio(by weight) | 2 | 1 |
Hardness(Shored) | 75-80 |
Operation time(100g mixed glue ,25ºC) | 50-60minutes |
Curing Time(25ºC) | 24-26hours |
Curing Time(35ºC) | 8hours |
Curing Time(25ºC) | 6-12months |
Feature
Epoxy resin HF402 can be cured under normal temperature and elevated temperature, with good flowing property, natural defoaming, high hardness, no ripple, bright in surface.* No Toxic Organic Compounds or Heavy Metals
* 100% Solids, Low VOC, Low odor,UV resistant
* Self-Leveling and Extremely Durable
* Crystal Clear, High Gloss and Excellent Color Stability
*Not whitish, no bubbles
*Anti-yellow for at least five years
*Food grade resin
Free samples are available! Please contact us for more details and tell us what you need!
Free samples are available! Please contact us for more details and tell us what you need!How to useStep 1: The ideal working temperature is around a constant 77°F. Best results can be obtained at constant temperatures between 70°F and 85°F, in a clean, dry, dust-free environment. Avoid working in high humidity. We recommend using this product on a leveled and flat work surface.
Step 2: Measure product in accordance with your intended use. Prepare 2 parts Base Resin to 1 part Curing Agent by liquid volume.Pour the Curing Agent first and then the Base Resin into a clean, smooth-sided container large enough to hold all the liquid and allow room for mixing.
Step 3: The material must be mixed thoroughly for at least 3 minutes. Be sure to scrape the container sides, bottom, and corners as you mix. Be careful not to whip excessive air into the mixture. If mixing a gallon, use a power mixer set to "hand speed." For smaller quantities, use stir sticks. Do not mix more than a gallon. Pour into a new, clean container and mix for an additional minute.
Step 4: Pour the mixed resin onto the surface and distribute evenly with a squeegee or gloved hand. Continue to pour remaining material to achieve the desired thickness, allowing the resin to flow evenly over the project's sides. Resin can be poured up to 1/4" thick per pour.
Step 5: Use a heat source such as a heat gun to remove any bubbles by adding a small amount of heat to the surrounding area. The bubble will rise to the surface and pop.
Step 6: If you are going to make a second pour, the first pour should still be slightly sticky. Once the second pour is made, bubbles may once again need to be removed. Material will feel hard after 45-60 minutes, cure to the point of workability within 24 hours, but full cure and maximum hardness can require up to 7 days, depending upon the temperature.Company Profile:
Shanghai Guanru Chemical Co., Ltd. is a high-tech enterprise focusing on chemical R&D, production, sales and technical services. It is determined to provide global customers with high-quality products, professional technical support, and efficient and high-quality services. Guanru Chemical can provide global customers with products and solutions in various fields such as pulping&paper-making industry, textile printing and dyeing industry, architectural coatings industry, water treatment industry and etc.Company Certificates: Shanghai Guanru Chemical Co.,Ltd.