Item | Unit | Guarantee value | Guarantee value |
Max grain size | mm | 0.8 | 0.8 |
Bulk density | g/cm3 | ≥1.70 | ≥1.73 |
Specific resistance | μΩ.m | ≤8.5 | ≤8.0 |
Bending strength | MPa | ≥10.0 | ≥12.0 |
Compressive strength | MPa | ≥24.0 | ≥31.0 |
Thermal Condcutivity | W/(m.k) | ≥120 | ≥130 |
C.T.E.(100-600) °C | 10-6/°C | ≤2.5 | ≤2.5 |
Ash content | % | ≤0.3 | ≤0.3 |
High Pure Graphite | ||||
Item | Unit | baked twice | baked three time | baked four time |
impregnated once | impregnated twice | Impregnated three times | ||
grain size | mm | ≤325mesh | ≤325mesh | ≤325mesh |
Bulk density | g/cm3 | ≥1.68 | ≥1.78 | ≥1.85 |
Specific resistance | μΩ.m | ≤14 | ≤14 | ≤13 |
Bending strength | MPa | ≥25 | ≥40 | ≥45 |
Compressive strength | MPa | ≥50 | ≥60 | ≥65 |
Ash content | % | ≤0.15 | ≤0.1 | ≤0.05 |
Item | Unit | Isostatic graphite |
grain size | μm | 5-22 |
Bulk density | g/cm3 | 1.75-1.85 |
Specific resistance | μΩ.m | 10-15 |
Bending strength | MPa | ≥40 |
Compressive strength | MPa | ≥70 |
Shore hardness | ≥5 | |
C.T.E.(100-600) °C | 10-6/°C | 3.2-5.2 |
Modulus of elasticity | GPa | 9.5-12.5 |