Project name | At the same level of ordinary concrete | Steel Fiber Reinforced Concrete | Growth rate |
C30(RC) | C30(SFRC) | ( % ) | |
Tensile Strength | 3.5MPa | 5.39-7MPa | 54-100 |
Compressive strength | 31.2MPa | 32.5-40MPa | 4.4-28.2 |
Ultimate bending strength | 5.5MPa | 9.18-13.75MPa | 67-520 |
First cracking strength | 4.88MPa | 7-8Mpa | 43-100 |
First-crack strength | 8.85N.m | 23-53N.m | 160-500 |
Impact fatigue limit | 5.96/cm2 | 53.3-91/m2 | 8-15 Time |
Impervious grades | P4 | P6~p12 | 0. |