Prevent The Embrittlement of The Elastic Fibers Textile Auxiliaries Lycra Protector Gr-L101

Min.Order: 500
Product origin: Zibo, Shandong, China
Infringement complaint: complaintComplaint
US$ 2 ~ 2.5

Description


Zibo Green New Material Technology Co., Ltd is established in 2010, located in Zibo city, Shandong Province, China.
Has own formulation and R&D group to develop the products.
Our products have been widely exported to the world with excellent quality and service, establish long-term business relationship with customers in Bangladesh, Vietnam, India, Singapore, Philippines, Korea, Sri Lanka, Cambodia and other countries in the World.
We not only sales products, but provide advanced technology support.!

 
Product Description

 

Lycra Protector GR-L101


Recommend technology in denim washing process

1. Desizing process:
Add GR-L101 0.5g/L (500g/machine), soap oil HP6, 0.2-0.5g/L, warmed to 50-60ºC, run 8-10 minutes, then drain cleaning.

2. Enzyme Washing process:
GR-L101, 0.2g/L (200g/machine), warmed to required temperature 40-50 ºC (or without warm), add acid or neutral cellulase (powder or liquid), adjust pH value in advanced if use acid cellulase. Washing time be based on sample plate requirement, drain cleaning after right edition.

3. Sodium hypochlorite bleaching process:
Caustic soda, 0.5-1g/L ( 500-1000g/machine, only add when heavy bleaching); spandex protector GR-L101, 1-1.5g/L (1000-1500g/machine) before adding bleaching liquor, add GR-L101, run for 3-5 minutes, warm up while running, add bleaching liquor to 50ºC in batches, add 1/5 bleaching liquor for the first time, run for a few minutes, add the remaining 4/5 bleaching liquor for the second time, according to the specific process time drift, drain liquor while flooding water after bleaching be finished, washed for 3 minutes, add dechlorination deodorant 0.3-0.5g/l, 25 ºC ×5-10min dechlorination treatment, water washing, dehydration and drying.



 
Application

Application on garment dyeing

1. H2O2 bleaching technology:

Caustic Soda2-3g/L
H2O2 (35%)7-15g/L
GR-L1011-2g/L
Temperature-Time80-85ºC×60-120 min
Bath ratio1:10-20


2. Dyeing process:


    Add GR-L101 in advanced, 1-2g/L, run 3 minutes, treated as normal dyeing process, can reach uniform dyeing, and bright color effect, and certain and certain deepening effect.




 