1, Properties:
PP fibre Undee/ wave form can be instead of steel fibre in cement concrete for anti-crack. Easy to disperse and construct.
2, Application:
Suggestion of Additive rate: 5.4kg fibre in one cubic meter concrete. (not less than 2.7kg/M3)
Technic of mixture:
Put the fibre into detritus first, then put grit to mix for about 2minutes, to make the fibre be dispersed. Then put cement and water to mix as per normal technic.
SPECIFICATION:
Raw Material----------------PolypropyleneFiber Type-------------------wave formFiber Dia. --------------------0.9±0.1mmMelting Point(ºC)---------- 160-170Acid &Alkali Resistance --Strong
Crack Elongation -----------15-20%
Elastic Modulas (MPa) ----5192
Tensile Strength(MPa) 450-700