Tensile Strength | MPa | 20.5 |
Fracture Tensile Strain | % | 320 |
Ageing Temperature | ºC | 100 |
Ageing Time | h | 168 |
Tensile Strength After Ageing | MPa | 22.5 |
Max Change of Tensile Strength | % | +12 |
After Ageing Fracture Tensile Strain | % | 290 |
Max Change of Fracture Tensile Strain | % | -10 |
Thermal Deformation | % | 28 |
Thermal Ageing Quality Loss | g/m² | 19 |
200ºC Thermal Stability Time | min | 90 |
20ºC Volume Resistivity | Ω.cm | 2.0*1011 |
Tensile Strength | MPa | 20 |
Fracture Tensile Strain | % | 330 |
Ageing Temperature | ºC | 100 |
Ageing Time | h | 240 |
Tensile Strength After Ageing | MPa | 21.5 |
Max Change of Tensile Strength | % | +8 |
After Ageing Fracture Tensile Strain | % | 310 |
Max Change of Fracture Tensile Strain | % | -6 |
Thermal Deformation | % | 28 |
Thermal Ageing Quality Loss | g/m² | 9 |
200ºC Thermal Stability Time | min | 120 |
20ºC Volume Resistivity | Ω.cm | 2.0*1010 |