Waterproof HDPE Geomembrane Plastic Pond Liner UV Resistant for Ponds Hot Sell

Min.Order: 5,000
Product origin: Tai'an, Shandong, China
Infringement complaint: complaintComplaint
US$ 0.6 ~ 0.8

Description

1.Introduction:


HDPE Geomembrane made from polyethylene polymer materials, through blowing or extruding technology, CE/ASTM/GB standards available. Our thickness ranges from 0.2-3mm; smooth, textured or bi-color surfaces available. HDPE Geomembrane main function is to prevent the liquid leakage and gas volatile. It is widely used in lining of pond reservoirs, canal, waste water, landfill, dams, Lakes, fish ponds and many other areas because HDPE Geomembrane is cost effectiveness and resistance against chemical and weather conditions.
By the way, except HDPE Geomembrane, we can also produce LDPE/EVA/PVC/EPDM materials geomembranes.


2.Our advantages:

New raw material and the precise formula;
Advanced equipment, perfect production process;
Real-time detection, strict quality control staff;
The packaging is solid to ensure the safety of the goods in delivery.

3.Application:


1. Prevent leakage disposal in landfills, waste water, or in waste dregs disposing field.
2. Retain river bank, lake dam, mine, reservoir, tunnel. Working as liquid storage pools.
3. Prevent leakage in subway, basement, tunnel. Also, it prevents anti-salt leakage in roadbed, and other projects.
4. The plane and the vertical direction laying of dam and ground sill, LLDPE Geomembrane Liner is used in the construction fence and waste material fields.
5. Used in ground sill of road, highway, railway, and waterproof layer of swelling clay.
6. Prevent leakage on rooftop.
HDPE Geomembrane: (ASTM/CE/GB standards available)  
Thickness/mm0.7511.251.522.53
Lowest Individual of 10 values / Nom.(mil)-10%
Density / min. g/cc0.94-0.96
Yield Strength KN/M11151822293744
Break Strength KN/M20273340536780
Yield Elongation %12
Break Elongation %700
Tear resistance/N93125156187249311374
Puncture Resistance/N240320400480640800960
Stress Crack Resistance (hr.)500
Carbon Black Content (%)2-3
Carbon Black DispersionNote(4)
Oxidative Induction Time(OIT)(min.ave.) (5)
  1. Standard OIT
  2. High Pressure OIT
100min.
400min.
Oven Aging at 85ºC (5).(6)
  1. Standard OIT (min.ave.) -% retained after 90 days
  2. High Pressure OIT (min.ave.) -%
retained after 90 days
55%
80%
UV Resistance (7)
  1. Standard OIT (min.ave.)
(b)High Pressure OIT (min.ave.) -%
retained after 1600 hrs (9)
1/2/3.95/4/5.5/6
MarksSmooth or texture surfaces available;
HDPE/LDPE/PVC materials available
FAQ:
 
Q: Are you factory or trading company?
A:  We are factory direct sale.

Q: Which country did you export?
A: Our products have been exported to many countries all over the world, including USA, Panama, Colombia, Chile, Peru, Ecuador, Russia, UK, Italy, France, Germany, Poland, Hungary, Turkey, Romania, Israel, India, Philippines, Singapore, Vietnam, Thailand, Indonesia, Australia, New Zealand...
 
Q: May I have your samples for testing?
A: Yes. We are glad to provide free samples within 5 days. Usually we provide A4 size free sample. New Client needs to pay the air delivery cost.
 
Q: What is your MOQ?
A: Normally, MOQ is one 20'GP container. But we also accept LCL for trial order.
 