Item | Specs | Test Method |
Shore Hardness(Asker C) | 17-23 | ASTM D2240 |
Density( KG/M3) | 140±20 | ASTM D3574 |
Tens Tensile Strength(Mpa) | ≥0.6 | ASTM D412 |
ElongationRate(%) | ≥150 | ASTM D412 |
Tearing strength (kn/m) | ≥2..5 | ASTM D624 |
Flame Retardant Rating | ≤100mm/MIN | |
Water Absorption (%) | ≤2 | ASTMD1056 |
Shrinkage (70ºC 24HRS )(%) | ≤3 | ISO 188 |