Rongxing-made Semi-coke is light black, characterized by high fixed carbon, high specific resistance, high chemical activity, low ash content, low sulfur and Low phosphorus. It is wildly applied to such industries as chemical industry, metallurgic industry and gas- making industry. Application of Semi Coke Be used in blast furnace instead of coal injection in steel-making. 0-6mm semi coke: sintering Mn ore in process of production SiMn; or using in other sinter mill. 6-18mm semi coke: producing Ferronickel , Ferrosilicon ,Calcium Carbide and other ferroalloy. |
Size | 18-30mm |
Fixed Carbon | ≥83% |
Ash | ≤8% |
Sulphur | ≤ 0.40%-0.50% |
Moisture | 10-15% |
Phosphorus | ≤0.012% |
w(k+Na) | ≤0.2% |
Advantage of semi coke in Ferro-alloy smelting
*High fixed carbon (84% min)
*Low ash (9% max)
*Low Phosphorus (0.03% max)
*Low Sulfur (0.4%max)
*High specific resistance
*High chemical activity
*High conductivity to lower the electric power
*Reduce pollution
Introduction of Rongxing Group-Semi Coke Supplier Founded in 1992, Rongxing Group is China's leading sullpier focusing on the research, development, production and sales of semi coke and other industry peoducts. Since the establishment of the company, following the development concept of "technology, environmental protection, energy saving, high quality of products", it has innovation in the traditional semi coke production industrial technology. After technological upgrading, the company has now entered the fast track of development, and its semi coke products are exported to Asia, Europe, Africa, South America and Oceania, which enjoys good reputation. We understand that your biggest demand is high quality , fast delivery and competitive price. we firmly believe that we can become your reliable partner for a long time once we start our cooperation. Supply: to any bulk port terminal with coke handling and storage facility Rongxing Capacity to supply annually: 100,000+ metric tons annually Markets: Asia, Europe ,Africa, South America and Oceania |
Sepecial Notes for semi coke 1. The height and diameter of the chimney must be ensured, and the chimney interface and the chimney itself must not leak (the chimney is too low or too thin will cause the heating furnace to not burn normally, seal the fire and extinguish the fire, etc.). 2. Adjust the size of the air inlet on the dust removal door according to the situation when sealing the furnace, to prevent the situation that the fire can not be sealed or extinguished when the furnace is sealed. 3. If a chimney hat is added, the hat should be more than 50cm away from the mouth of the chimney. |