Product Classification:Titanium alloy |
Material:TC4 |
Product introduction: |
It is composed of Ti-6Al-4V and belongs to (α+β) type titanium alloy, which has good comprehensive mechanical and mechanical properties. The specific strength is greater. TC4 has a strength sb=1.012GPa, a density g=4.51g/cm3, and a specific strength sb/g=23.5, while the specific strength sb/g of alloy steel is less than 18. Titanium alloys have low thermal conductivity. The thermal conductivity of titanium alloy is 1/5 of iron and 1/10 of aluminum, and the thermal conductivity of TC4 is 7.955W/m·K. |
Chemical Composition: |
Ti | Fe | C | N | H | O | Al | V |
Allowance | ≤0.30 | ≤0.10 | ≤0.05 | <0.015 | ≤0.20 | 5.5~6.8 | 3.5~4.5 |
Physical Properties: |
Density g/cm3 | Tensile strength σb/MPa | Elongation stress σr0.2/MPa | Elongationδ5(%) | Reduction of section ψ(%) |
4.5 | ≥895 | ≥825 | ≥10 | ≥25 |
Application field: |
Aerospace, petrochemical, shipbuilding, automobile, medicine and other departments |
The composition of TC4 titanium alloy is Ti-6Al-4V, belonging to( α+β) Type titanium alloy with excellent comprehensive mechanical and mechanical properties. Greater than strength. The strength of TC4 is sb=1.012GPa, density g=4.51g/cm3, and specific strength sb/g=23.5, while the specific strength sb/g of alloy steel is less than 18. Titanium alloy has low thermal conductivity. The thermal conductivity of titanium alloy is 1/5 of iron and 1/10 of aluminum, and the thermal conductivity of TC4 is l=7.955W/m · K. |
|
|
|
|
|
|
|