El tema | 
Criterios de Prueba | 
Unidad | 
Valor |

Grosor | 
Superficie de contacto | 
Um | 
80 |

Fuerza tensil | 
MD | 
La norma ASTM D882 | 
MPa | 
39 |

TD | 
35 |

La elongación | 
MD | 
La norma ASTM D882 | 
% | 
323 |

TD | 
383 |

Resistencia a la ruptura tangencial | 
MD | 
La norma ASTM D1938-67 | 
N/cm. | 
122.8 |

TD | 
100.5 |

OTR | 
La norma ASTM D3985(20° C65%RH) | 
C m3/m2 de la barra. D. | 
60 |

WTR | 
La norma ASTM E96(40° C90%RH) | 
G/m2. | 
1.5 |

Haze | 
La norma ASTM D1003 | 
% | 
5 |

La transparencia | 
MD | 
La norma ASTM D1894 | 
 | 
0.37 |

TD | 
 |

Tensión de la húmeda | 
La norma ASTM D2578 | 
Mn/m. | 
40 |