Bulletproof feuille propety plaque en acier | ||||||||
Grade | Plage d'éPaisseur (mm) | La dureté | RéSistance àLa traction | La force de rendement | Enlogation | 90ºCold essai de flexion | ,-20valeur ºImpact,KV2(J) | |
BHFD3 (PRO500) | 2.0-120 | 470-550HB | Min 1250Mpa | Min 1100Mpa | Min 7 % | R>=8T | >=10 | |
La Composition chimique (%) | ||||||||
C | Si | Mn | P | S | Cr | Mo | Ni | B |
<=0,36 | <=1,70 | <=2,20 | <=0,02 | <=0,015 | <=0,70 | <=0,50 | <=0,60 | <=0.0050 |